Re: TRANNY CASE CRACKED!!!! weld the crack? or jb weld???
Originally Posted by crxmatt2
if you JB welded it.. since you're selling the car, would you tell a potential buyer that you JB welded the trans case? You better tell them or you'll be considered a SCAMMER by our fellow hmt community...
ofcourse the car will never sell now.. it seems like the dripping has stopped.. so idk where the ---- that oil came from yesterday before going to bed i took a newspaper stretched it out over cardboard and taped it on and stuck it under the tranny.. i just checked it today and it was clean.. so idk wtf is up..
Originally Posted by ichbinsobose
:P
Cover the final concotion with "automotive goop" like a whole tube, wont drip through without pressure. Youll have enough to cover like 3 square feet. |
Re: TRANNY CASE CRACKED!!!! weld the crack? or jb weld???
A minor crack with jb weld on it and can be driven till the end of time. A blown headgasket has the car down for days and machine shop costs
|
Re: TRANNY CASE CRACKED!!!! weld the crack? or jb weld???
selling my baby for 1900 :(
guy coming to pick it up :( |
Re: TRANNY CASE CRACKED!!!! weld the crack? or jb weld???
Originally Posted by jay
selling my baby for 1900 :(
guy coming to pick it up :( atleast you got some cash now |
Re: TRANNY CASE CRACKED!!!! weld the crack? or jb weld???
Originally Posted by chris
atleast you got some cash now that way when i start my gsr and drive it.. and if there really is a washer in it.. i can shut it off and then have fun swapping/mixing and matching gsr/b16 gears lsd tranny yay cant wait... im only going to put it into gear and roll slowly till i hear the tranny make noises then shut it down.. fkn A |
Re: TRANNY CASE CRACKED!!!! weld the crack? or jb weld???
weld :y
|
Re: TRANNY CASE CRACKED!!!! weld the crack? or jb weld???
crx sold.. guy says he will give me my old tranny.. hopefully this is true..
oh well |
Re: TRANNY CASE CRACKED!!!! weld the crack? or jb weld???
Originally Posted by jay
crx sold.. guy says he will give me my old tranny.. hopefully this is true..
oh well hope so you have like one of the last y1 lsd transmissions in the us |