Re: TRANNY CASE CRACKED!!!! weld the crack? or jb weld???
Originally Posted by Ravage70
90% of muffler shops dont touch Aluminum
|
Re: how can i open my gsr tranny... bad fucking luck...
Originally Posted by JoshMO
meh look at it this way. When your shitty ass luck finally takes a turn for the better you'll at least have a lot more knowledgeablities under your belt there, buk
|
Re: TRANNY CASE CRACKED!!!! weld the crack? or jb weld???
Originally Posted by buk9tp
jb weld it is :y
CLEAN THAT ---- GOOD and I mean grind into the crack a bit if you can. Make it as clean and rough as possible and you should be golden. |
Re: TRANNY CASE CRACKED!!!! weld the crack? or jb weld???
JB weld nugga do it. I heard that it can heal diabetes too. True story
|
Re: TRANNY CASE CRACKED!!!! weld the crack? or jb weld???
Originally Posted by JoshMO
JB weld nugga do it. I heard that it can heal diabetes too. True story
|
Re: TRANNY CASE CRACKED!!!! weld the crack? or jb weld???
well.. i went ahead and did the first coat.. i used a spoon to apply it on then a Q tip and tooth picks to get it into all the little cracks..
the cotton on the qtip broke off so i let it stay in the jb weld.. figured it would act like fiberglass.. too late now to get it out ah well.. next coat is gonna be even bigger.. + the aluminum like chris said i dont think this ---- is going anywhere.. lol |
Re: TRANNY CASE CRACKED!!!! weld the crack? or jb weld???
You Big daddy scruff:
The M2B4 tranny that has miraculously survived in my pile of mess thus far had a hole the size of a car key in the bellhousing from a bolt going IN TO the tranny from the outside. I cleaned the ---- out of it with brake clean, ground the edges, hit it with acetone and welded a piece of aluminum into the hole... then jb welded over the top of that JUST TO BE SURE it wouldnt leak.... I havent had any issues with it yet. As long as the crack isnt in an area that carries funky loads (IE bearing boss or the like) thats going to be compromised you ll be fine. mine was right behind the pressure plate on the thin thin part of the case so I got KIND of lucky.... The alloy the case is made out of is shitty to start with so its a fucker to weld (its really pourus and low quality).... it can totally be done, but someones gonna have to know how to tig/heliarc fairly well JB weld will be fine if its not in a structuraly dependant area |
Re: TRANNY CASE CRACKED!!!! weld the crack? or jb weld???
fkn A
went out there this morning and there were drops of oil forming arround the outside of the jb weld.. i was pissed because the tranny drained pretty ------- good.. idk where the ---- the oil came from.. i said ---- it.. hosed it with brake cleaner.. sanded the ---- outta the jb weld to rough it up.. mixed up a big ass batch of jb weld and poured it into some aluminum foil then smashed it into the area arround the crack/bolt plan is to peel off any loose foil when its tried out sand it down.. then give it one last coat.. then sand it down and spray paint it.. lol yeah.. this fucker better not leak.. |
Re: TRANNY CASE CRACKED!!!! weld the crack? or jb weld???
:P
Cover the final concotion with "automotive goop" like a whole tube, wont drip through without pressure. Youll have enough to cover like 3 square feet. |
Re: TRANNY CASE CRACKED!!!! weld the crack? or jb weld???
if you JB welded it.. since you're selling the car, would you tell a potential buyer that you JB welded the trans case? You better tell them or you'll be considered a SCAMMER by our fellow hmt community...
|